  1. Abstract: Porosity of die castings caused by air entrapped into the liquid metal in the shot sleeve is common problem of die csating process.
    文摘:压室中气体卷入金属液内而造成压铸件内部气孔是压铸过程常见的问题。
  2. Working state of shot sleeve is analyzed, further more according to my own experience some new design methods are proposed.
    分析了压室的工作状况,进而根据自己的经验提出几种新设计方法。
  3. The air entrapment of the liquid metal flow in the shot sleeve during the slow shot phase is one of the factors resulting in this kind of defect.
    气孔是压铸生产中的常见问题,导致这一缺陷的原因之一就是在慢压射过程中压室内的金属液流动卷入了气体。
  4. 2-D Simulation of Temperature Distribution and Deformation in Shot Sleeve of Die Casting Machine
    压铸机压室温度分布与变形的二维模拟
  5. The numerical simulation for liquid metal flow in the shot sleeve and heat transfer was performed by the developed model. The simulated results is well in agreement with the Flow-3D simulated ones and critical velocity.
    采用所开发的模拟程序对压室金属流动及传热过程进行了模拟,模拟结果与FLOW-3D的计算结果以及临界速度理论作比较,两者均吻合。
  6. 3D Numerical Simulation of Temperature Field Coupled with Flow Field of the Liquid Metal in Shot Sleeve of Die Casting Process
    压室液态金属流动耦合温度场三维数值模拟
  7. Based on numerical simulation for mold filling of die casting process, the moving boundary condition was introduced to deal with the movement of the plunger and to simulate the flow field in the shot sleeve.
    文中在压铸流场模拟的基础上,增加了移动边界条件处理冲头的移动过程,模拟了慢压射过程中压室内流体的流动形态。
  8. The bottom of shot sleeve is filled with melt by horizontal cold chamber die casting machine, when the beginning of the slow shot phase, volume on the melt to the top of sleeve is occupied by gas.
    卧室冷室压铸机压铸时,压室底部被浇入的金属熔体所覆盖,熔体上部分至压室顶部的空间被气体所占据。